CATALOGUEC72900
Copper-Nickel-Tin Alloy
High-strength Cu-Ni-Sn alloy for load-bearing sliding and wear-sensitive components.
View technical data ↗An engineering Cu-Ni-Sn option for elastic elements and demanding parts requiring a balance of properties.
Catalogue material image.
Reference values: Brochure grades include C72500 (YWF92); properties depend on condition.
| Cu | Balance |
|---|---|
| Ni | 9 wt% |
| Sn | 2 wt% |
| Mn | ≤0.2 wt% |
| Zn | ≤0.5 wt% |
| Fe | ≤0.6 wt% |
| Property | SI | Imperial |
|---|---|---|
| Density | 8.90 g/cm³ | 0.322 lb/in³ |
| Electrical conductivity | 11 % IACS | — |
| Thermal conductivity | 48 W/(m·K) | 28 BTU/(hr·ft·°F) |
| Melting point | 960 °C | 1760 °F |
| Linear thermal expansion | 16.6 µm/(m·K) | — |
| Elastic modulus | 137 GPa | 19.87 Msi |
Applicable only to the listed diameter and condition. UTS: ultimate tensile strength; YS: yield strength.
| Condition | Diameter (mm) | UTS (MPa) | YS (MPa) | Elongation (%) | Hardness |
|---|---|---|---|---|---|
| M3-340 | Ø25–100 | 340–410 | ≥250 | ≥30 | 75–110 HV |
| H-380 | Ø25–100 | 380–470 | ≥200 | ≥10 | 110–150 HV |
| H-450 | Ø25–100 | 450–530 | ≥370 | ≥6 | 140–170 HV |
| H-500 | Ø25–100 | 500–580 | ≥450 | ≥3 | 160–190 HV |
| H-560 | Ø25–100 | 560–650 | ≥520 | ≥2 | 180–210 HV |
| H-610 | Ø25–100 | ≥610 | ≥580 | Not stated | >190 HV |
Round bars
Made to order / stock on inquiry · Price on request
The enquiry form will carry this grade automatically.
Request a Quote — C72500 ↗
CATALOGUECopper-Nickel-Tin Alloy
High-strength Cu-Ni-Sn alloy for load-bearing sliding and wear-sensitive components.
View technical data ↗
ILLUSTRATIVECopper-Nickel-Tin Alloy
Additional Cu-Ni-Sn grade option available for specification-based discussion.
View technical data ↗
CATALOGUECopper-Nickel-Tin Alloy
A Cu-Ni-Sn family option for mechanical and wear-related engineering applications.
View technical data ↗